This document specifies a method of converting room temperature percentage elongations after fracture obtained on various proportional and non-proportional gauge lengths to other gauge lengths.
Formula (1), on which conversions are based, is considered to be reliable when applied to carbon, carbon manganese, molybdenum and chromium molybdenum steels within the tensile strength range 300 N/mm2 to 700 N/mm2 and in the hot-rolled, hot-rolled and normalized or annealed conditions, with or without tempering.
These conversions are not applicable to:
a) cold reduced steels;
b) quenched and tempered steels;
c) austenitic steels.
These conversions are not applicable when the gauge length exceeds or where the width to thickness ratio of the test piece exceeds 20.
Označení | ČSN EN ISO 2566-1 (420308) |
---|---|
Katalogové číslo | 514429 |
Cena | 440 Kč440 |
Datum schválení | 1. 6. 2022 |
Datum účinnosti | 1. 7. 2022 |
Jazyk | angličtina (obsahuje pouze anglický originál), připravuje se převzetí v češtině |
Počet stran | 48 stran formátu A4 |
EAN kód | 8596135144297 |
Norma byla zrušena k | 1. 10. 2022 |
a nahrazena | ČSN EN ISO 2566-1 (420308) |
Tato norma nahradila | ČSN EN ISO 2566-1 (420308) z srpna 2000 |
Dostupnost | skladem (tisk na počkání) |
ČSN EN ISO 2566-2 (420308)
Ocel - Přepočet hodnot tažnosti - Část 2: Austenitické oceli